<p>The present invention lowers the strength before nitriding to improve the machinability, while deepens the effective hardened case of the nitrided case for improving the fatigue strength. It provides steel for nitriding use containing, by mass%, C: 0.05 to 0.30%, Si: 0.003 to 0.50%, Mn: 0.4 to 3.0%, Cr: 0.2 to 0.9%, Al: 0.19 to 0.70%, V: 0.05 to 1.0%, and Mo: 0.05 to 0.50%, having contents of Al and Cr satisfying
0.5%‰¤1.9Al+Cr‰¤1.8%, and having a balance of Fe and unavoidable impurities.</p> |