摘要 PROBLEM TO BE SOLVED: To modify steel slag at low costs in a short time, without transfer, as it is at high temperatures.SOLUTION: Steel slag in a molten state is kept in high-temperature water of 50°C or higher for a specified time to modify it, and the steel slag of grain sizes of 30 mm or smaller is recovered. Preferably, the steel slag in a molten state is reduced in grain sizes, poured into the high-temperature water and kept in the high-temperature water for a specified time to modify it. The grain sizes may be reduced to 10 mm or smaller by causing water to collide with the steel slag in a molten state, or the grain sizes may be reduced to 5 mm or smaller by causing a gas to collide with the steel slag in a molten state. The procedure allows modification of the steel slag at low costs in a short time, without transfer, as it is at high temperatures.
申请公布号 JP2015189602(A) 申请公布日期 2015.11.02
申请号 JP20140066431 申请日期 2014.03.27
申请人 JFE STEEL CORP 发明人 KATO YUSUKE;MIYATA YASUTO;MATSUNAGA HISAHIRO;HAYASHI AKIO
分类号 C04B5/00;C21B3/06;C21B3/08;C21C5/28;F27D15/00 主分类号 C04B5/00
代理机构 代理人
主权项
地址