摘要 |
<p>PROBLEM TO BE SOLVED: To provide a sinter member for a slide, which is excellent in wear resistance, oxidation resistance, and seizure resistance under a hot temperature environment.SOLUTION: Provided is the sinter member in which hard particles having 500 or more and 1800 or less of micro Vickers hardness are dispersed in an iron aluminide alloy. A content of the hard particles may be 5 volume% or more and 45 volume% or less. The particle diameter of each of the hard particles may be 20μm or more and 150μm or less. The Al content in the iron aluminide alloy may be 12 mass% or more and 35 mass% or less.</p> |