发明名称 |
Process for providing noble metal-containing mixtures for recovering noble metals |
摘要 |
The invention relates to the provision of noble metal-containing mixtures for a process for processing them by heating the mixture, preferably for processing them by means of an ashing process. This provision is characterized by the following measures: (a) moistening of the noble metal-containing mixture to be processed, (b) introduction of the moistened noble metal-containing mixture into at least one container which serves as diffusion barrier for water, and (c) introduction of the loaded container into a heat-resistant chamber together with at least one upper refractory mat. The noble metal-containing mixture is preferably moistened in the presence of a porous material and the chamber is closed by means of a heat-resistant covering. The invention further provides a processing process comprising the provision of noble metal-containing mixtures and also the heat-resistant chamber loaded with noble metal-containing mixtures itself. The process of the invention enables simple, clean recovery of noble metals in high yield from noble metal-containing mixtures. |
申请公布号 |
US9169536(B2) |
申请公布日期 |
2015.10.27 |
申请号 |
US201214111416 |
申请日期 |
2012.04.12 |
申请人 |
UMICORE AG & CO. KG |
发明人 |
Zimmermann Klaus;Hartmann Robert;Kinz Oswald;Grehl Matthias |
分类号 |
C22B11/02;F23G7/00 |
主分类号 |
C22B11/02 |
代理机构 |
Smith, Gambrell & Russell, LLP |
代理人 |
Smith, Gambrell & Russell, LLP |
主权项 |
1. Provision of noble metal-containing mixtures for a process for processing noble metal-containing mixtures by heating the mixture, wherein the provision comprises:
moistening of the noble metal-containing mixture to be processed, wherein the noble metal-containing mixture has a total water content in the range from 5 to 80% by weight, introduction of the moistened noble metal-containing mixture into at least one container to form a loaded container, wherein the at least one container serves as a diffusion barrier for water, introduction of the loaded container into a heat-resistant chamber together with at least one upper refractory mat, wherein the at least one upper refractory mat covers the loaded container. |
地址 |
Hanau-Wolfgang DE |