发明名称 |
Lithium manganese composite oxide and method for preparing same |
摘要 |
The present invention relates to a lithium manganese composite oxide and a method for preparing the same, and more particularly, to a lithium manganese composite oxide and a method for preparing same, in which a wet-milling process and a spray-drying process are applied, and the abundance ratio of Mn3+ ions to Mn4+ ions at the surface of the composite oxide is adjusted by controlling an oxidizing atmosphere during heat treatment. |
申请公布号 |
US9171653(B2) |
申请公布日期 |
2015.10.27 |
申请号 |
US201113883653 |
申请日期 |
2011.11.07 |
申请人 |
POSCO ES MATERIALS CO., LTD. |
发明人 |
Ko Hyoung-Shin;Kim Tae-Won |
分类号 |
H01B1/08;C01G45/12;C01G53/00;H01G11/04;H01G11/30;H01M4/131;H01M4/1391;H01M4/485;H01M4/505;H01M4/04;C01D15/02;H01M10/052 |
主分类号 |
H01B1/08 |
代理机构 |
Lucas & Mercanti, LLP |
代理人 |
Lucas & Mercanti, LLP |
主权项 |
1. A lithium manganese composite oxide comprising a compound represented by chemical formula 1,
wherein the compound represented by chemical formula 1 comprises Mn having an oxidation number of +3 and Mn having an oxidation number of +4, and the abundance ratio of Mn having an oxidation number of +3 to Mn having an oxidation number of +4 at the surface of the lithium manganese composite oxide, A, defined by relation formula 1, is 95 to 100:
Li1+aMn2−xMxO4 [Chemical Formula 1] wherein, a is 0 to 0.2, x is 0 to 0.4, and M is selected from the group consisting of Al, Mg, Zr, Cu, Ni, Sn, Sr, Zn, Si and a mixture thereof; and
A={Mn having an oxidation number of +4 abundance/(Mn having an oxidation number of +3 abundance Mn having an oxidation number of +4 abundance) }×100 [Relation Formula 1]. |
地址 |
Gumi-si, Gyeongsangbuk-do KR |