摘要 |
PROBLEM TO BE SOLVED: To provide a method for manufacturing an antiglare film, capable of promptly aggregating organic particles having an average particle size of 1 μm or more and 5 μm or less into a large aggregate.SOLUTION: An aggregate Y of organic particles is formed by: preparing a coating liquid including at least organic particles c having an average particle size of 1 μm or more and 5 μm or less, a water action thickening material a thickened by acting on water, a binder resin and an organic solvent; applying the coating liquid on a film base material into a wet film having a thickness of 10 μm or more; blowing a humid wind having a dew-point temperature of 10°C or more when the concentration of the solid content of the applied coating film T is 20 mass% or more and 60 mass% or less; and obliquely conveying the film base material at an angle of 10° or more and 60° or less to a horizontal plane after blowing the humid wind. |