摘要 [Object] To provide the manufacturing method for a copper and elemental copper free NAO friction material providing an excellent fade resistance and high mechanical strength. [Means to Resolve] This manufacturing method includes the mixing step of mixing the raw friction material compounds to obtain the raw friction material mixture, the kneading step to apply the raw friction material mixture in the sealed type kneader to knead while maintaining the melting temperature of the thermosetting resin in the kneader or higher but lower than the curing temperature under the predetermined pressure to obtain the kneaded raw friction material, the sizing step of sizing the kneaded raw friction material to obtain the raw friction material granulation article, and the hot press molding step of filling the raw friction material sized particles in the molding die to hot press molded by the press machine.
申请公布号 JP5797073(B2) 申请公布日期 2015.10.21
申请号 JP20110208899 申请日期 2011.09.26
申请人 日清紡ブレーキ株式会社 发明人 矢口 光明;本間 雅史;服部 恭輝
分类号 C09K3/14;F16D69/00;F16D69/04 主分类号 C09K3/14
代理机构 代理人
主权项
地址