摘要 A method for manufacturing a component having increased thermal conductivity through layer-by-layer construction. At least one section of the component is constructed by applying a layer section having predetermined dimensions of a composite material of a metal and/or a metal alloy and particles of a highly heat-conducting material, including diamond and/or cubic boron nitride, in a predetermined area on a base layer by melting the metal or the metal alloy a heat source, in such a way that the metal and/or metal alloy form(s) within the predetermined dimensions a cohesive matrix, in which particles of the highly heat-conducting material are embedded, and then cooling.
申请公布号 US9156058(B2) 申请公布日期 2015.10.13
申请号 US201313923120 申请日期 2013.06.20
申请人 EADS Deutschland GmbH 发明人 Brandl Erhard;Sander Joerg;Schoberth Achim
分类号 B32B5/16;B05D3/06;B22F3/105;C22C26/00 主分类号 B32B5/16
代理机构 Crowell & Moring LLP 代理人 Crowell & Moring LLP
主权项 1. A method for manufacturing a component having increased thermal conductivity through layer-by-layer construction, wherein least one section of the component is constructed by performing at least once a step comprising: a) applying a layer section having predetermined dimensions of a composite material of a metal and/or a metal alloy and particles of a highly heat-conducting material, comprising diamond and/or cubic boron nitride, in a predetermined area on a base layer by melting the metal or the metal alloy by a heat source in such a way that the metal and/or metal alloy forms, within the predetermined dimensions, a cohesive matrix in which particles of the highly heat-conducting material are embedded, and then cooling, wherein the metal of the metal and/or metal alloy is Al or Mg, and wherein a size of the particles of the highly heat-conducting material, comprising diamond and/or cubic boron nitride is in the range of approximately 6 μm to approximately 250 μm, wherein a size distribution is bimodal or trimodal.
地址 Ottobrunn DE