发明名称 A PROCESS FOR PRODUCING IRON ORE SINTER WITH IMPROVED REDUCTION DEGRADATION INDEX (RDI)
摘要 <p>A low reduction degradation index is desired in Iron ore sinter. Indian iron ore fines contain a high percentage of alumina and this has a deleterious effect of sinter quality, particularly RDI. This invention proposes a method for improving the RDI of sinter by increasing the CaO content and the suction pressure employed during sintering. This combination of sinter CaO and suction pressure helps in controlling RDI by increasing the amount of unassimilated hematite and decreasing the amount of secondary hematite present in sinter.</p>
申请公布号 IN395KO2014(A) 申请公布日期 2015.10.02
申请号 IN2014KO00395 申请日期 2014.03.26
申请人 TATA STEEL LIMITED 发明人 SRI HARSHA NISTALA;MANOJ KUMAR CHOUDHARY;MRIGANSHU GUHA;MONI SINHA
分类号 C22B1/00 主分类号 C22B1/00