发明名称 |
WET STRENGTHENED FIBER PRODUCTS, WET STRENGTHENING RESINS, AND METHODS FOR MAKING AND USING SAME |
摘要 |
Wet strengthened fiber products, wet strengthening resins, and methods for making such wet strengthened fiber products and wet strengthening resins. The wet strengthened fiber product can include a fiber web and an at least partially cured wet strengthening resin, which prior to at least partially curing, the wet strengthening resin can include a polyamide-epihalohydrin (PAE) resin and a cationic styrene maleimide (SMI) resin. The PAE resin can include a reaction product of a polyamidoamine and an epihalohydrin and the cationic SMI resin can include a reaction product of a styrene maleic anhydride (SMA) copolymer and an amine. The wet strengthened fiber product can include the wet strengthening resin in an amount of about 0.05 wt % to about 5 wt %, based on a dried weight of the wet strengthened fiber product. |
申请公布号 |
US2015275438(A1) |
申请公布日期 |
2015.10.01 |
申请号 |
US201514668097 |
申请日期 |
2015.03.25 |
申请人 |
Georgia-Pacific Chemicals LLC |
发明人 |
Hagiopol Cornel;Townsend David F.;Ringold Clay E.;Johnston James W. |
分类号 |
D21H21/20;D21H17/40;D21H17/55 |
主分类号 |
D21H21/20 |
代理机构 |
|
代理人 |
|
主权项 |
1. A wet strengthened fiber product, comprising:
a fiber web; and an at least partially cured wet strengthening resin, wherein, prior to at least partially curing, the wet strengthening resin comprises:
a polyamide-epihalohydrin resin comprising a reaction product of a polyamidoamine and an epihalohydrin; anda cationic styrene maleimide resin comprising a reaction product of a styrene maleic anhydride copolymer and an amine compound, a weight average molecular weight of about 500 to about 200,000, and a styrene to maleimide molar ratio of about 1:1 to about 5:1;wherein the cationic styrene maleimide resin is present in the wet strengthening resin in an amount of about 5 wt % to about 95 wt %, based on the combined weight of the polyamide-epihalohydrin resin and the cationic styrene maleimide resin; andwherein the wet strengthening resin is present in the wet strengthened fiber product in an amount of about 0.05 wt % to about 5 wt %, based on a combined weight of the polyamide-epihalohydrin resin and the cationic styrene maleimide resin relative to a dried weight of the wet strengthened fiber product. |
地址 |
Atlanta GA US |