摘要 |
<p>Disclosed herein is a method for preparing permanently hydrophobic aerogel and permanently hydrophobic aerogel prepared by the method. The method comprises adding sodium silicate to HCl at 30 to 90 °C until an acidity reaches pH 3-5, to form silica hydrogel under acidic conditions of pH 3-5, washing the silica hydrogel with distilled water using a mixer, followed by filtering, adding the silica hydrogel to a silylating solution of silylating agent in n-butanol at pH 1-5 using an acid selected from hydrochloric acid, sulfuric acid, phosphoric acid and nitric acid, to simultaneously conduct silylation and solvent replacement, and drying the silica hydrogel. The method has the following advantages; i) silylation and solvent replacement can be simultaneously conducted, ii) n-butanol is used as a reaction solvent instead of methanol upon silylation, thus obtaining a thermal conductivity comparable to conventional aerogel powders, iii) silylation is conducted under improved conditions, i.e., strong acidic conditions of pH 1-5, and as a result, all of the aerogel powders can be reacted with a silylating agent, thereby obtaining permanently hydrophobic aerogel, iv) the washing with a mixer makes the amount of removed sodium ions uniform, thus it is suitable for mass-production, and v) the method provides a relatively simplified procedure and the use of the silylating agent in a small amount enables low costs and mass-production.</p> |
申请人 |
KOREA INSTITUTE OF INDUSTRIAL TECHNOLOGY;KIM, GYUNG-SOO;CHUN, HYUN-AEE;CHOI, HYUN-CHUL;KIM, YOUNG-JUNG |
发明人 |
KIM, GYUNG-SOO;CHUN, HYUN-AEE;CHOI, HYUN-CHUL;KIM, YOUNG-JUNG |