发明名称 METHOD FOR PRODUCING ROLLING MEMBER, ROLLING MEMBER AND ROLLING BEARING
摘要 PROBLEM TO BE SOLVED: To provide a method for producing a rolling member, the rolling member and a rolling bearing, wherein a rolling fatigue service life, especially under severe circumference, such as high contacting surface pressure, is improved. SOLUTION: The method for producing the rolling member includes: a forming member preparing process for preparing the forming member composed of a steel containing by mass% of 0.6-1.2% carbon, 0.15-1% silicon, 0.3-1.5% manganese, 0.1-2% chromium and 0.1-2% vanadium; a carbo-nitriding process for carbo-nitriding the formed member at the temperature of A<SB>1</SB>point or higher; a first cooling process for cooling the formed member to the lower temperature than the A<SB>1</SB>point; a heating process for heating the formed member to the temperature of the A<SB>1</SB>point or higher and the lower temperature than the carbo-nitriding temperature; and a second cooling process for cooling the temperature of M<SB>s</SB>point or lower from the temperature of the A<SB>1</SB>point or higher. COPYRIGHT: (C)2007,JPO&INPIT
申请公布号 JP2007100127(A) 申请公布日期 2007.04.19
申请号 JP20050288016 申请日期 2005.09.30
申请人 NTN CORP 发明人 HAMADA HIROSHI;MATSUBARA YUKIO;MAEDA KIKUO
分类号 C21D9/40;C21D1/06;C22C38/00;C22C38/24;C22C38/46;F16C19/06;F16C19/28;F16C33/32;F16C33/34;F16C33/62;F16C33/64 主分类号 C21D9/40
代理机构 代理人
主权项
地址