A method of making a dial table (10) is provided. A foam layout (14) is interposed between a base assembly (18) and a top assembly (12) to form a composite layout. The base assembly (18) includes a first segmented carbon fiber layout therein and the top assembly (12) includes a second segmented carbon fiber layout therein. A caul plate (88) is then placed adjacent to the composite layout. The caul plate includes a plurality of caul plate apertures (92). A vacuum is thereafter generated proximate the composite layout. A resin is drawn through the plurality of caul plate apertures using the generated vacuum until the composite layout is infused with the resin. The caul plate is removed from adjacent the composite layout and the resin-infused composite layout is baked. Thus, the dial table is made.
申请公布号
WO2006096647(A3)
申请公布日期
2009.04.09
申请号
WO2006US07930
申请日期
2006.03.06
申请人
SCIENTIFIC COMPOSITES;BLAKELEY, ANTHONY;KELLY, DAN