摘要 |
PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition having a small linear expansion coefficient, high rigidity, and excellent surface appearance, and to provide a molded product thereof. SOLUTION: The thermoplastic resin composition is prepared by mixing: (A) an aromatic polycarbonate resin; (B) an aromatic polyester resin; (C) talc; and (D) carbon fiber. As for 100 wt.% of the sum of the aromatic polycarbonate resin (A) and the aromatic polyester resin (B), the amount of the aromatic polycarbonate resin (A) is 1-99 wt.% and the amount of the aromatic polyester resin (B) is 1-99 wt.%. As for 100 pts.wt. of the sum of the aromatic polycarbonate resin (A) and the aromatic polyester resin (B), the amount of talc (C) is 1-100 pts.wt. and the amount of carbon fiber (D) is 1-50 pts.wt. The molded product thereof is also provided. COPYRIGHT: (C)2011,JPO&INPIT
|