发明名称 BOUTEILLE EN ALUMINIUM POUR MELANGE GAZEUX NO/AZOTE
摘要 #CMT# #/CMT# The method involves providing a main body (1) that comprises an internal volume (7) with capacity ranging between 2 and 30 l. The main body is made of aluminum alloy including a mass proportion of lead lower or equal to 50 ppm, silicon between 0.1 and 1.5 percent, manganese lower than 0.5 percent, and magnesium between 0.1 and 2 percent. Mixture of nitric oxide/nitrogen with pressure greater than atmospheric pressure is introduced into the internal volume of a container i.e. steel bottle. #CMT#USE : #/CMT# Method for conditioning mixture of nitric oxide and nitrogen in a conditioning container for a newborn child suffering from primitive pulmonary hypertension or a patient undergoing heart surgery. #CMT#ADVANTAGE : #/CMT# The mixture of nitric oxide/nitrogen with the pressure greater than atmospheric pressure in introduced into the internal volume of the container, thus minimizing variation of capacity in the range of plus or minus 1.5 percent in the container, and allowing the container to be resistant to high pressure and shocks, and reducing weight of the container. #CMT#DESCRIPTION OF DRAWINGS : #/CMT# The drawing shows a sectional view of a packaging container containing nitric oxide and nitrogen gaseous mixtures. 1 : Main body 2 : Collar 3 : Container bottom 6 : Ground 7 : Internal volume #CMT#METALLURGY : #/CMT# The aluminum alloy includes 0.01 and 0.8 percent of chromium, between 0.001 and 1 percent of iron, 1 percent of copper, between 0.001 and 0.5 percent of zinc and/or 0.001 and 0.5 percent of tintanium.
申请公布号 FR2977297(B1) 申请公布日期 2015.01.16
申请号 FR20110055788 申请日期 2011.06.29
申请人 L'AIR LIQUIDE,SOCIETE ANONYME POUR L'ETUDE ET L'EXPLOITATION DES PROCEDES GEORGES CLAUDE;AIR LIQUIDE SANTE FRANCE;AIR LIQUIDE SANTE (INTERNATIONAL) 发明人 DE VILLEMEUR PIERRE;LECOURT LAURENT;LEVINSON BENEDICTE
分类号 F17C1/14 主分类号 F17C1/14
代理机构 代理人
主权项
地址