摘要 |
PROBLEM TO BE SOLVED: To provide a method of manufacturing an organic electronic device, which seals only an end part of an organic thin-film solar cell, is inexpensive, and has high manufacturing efficiency.SOLUTION: The method seals an end part of an organic thin-film solar cell having a substrate 1, an organic thin-film solar cell element 2, and a first barrier layer 3 in this order. In the method, a laminate of a second barrier layer 6 and a barrier adhesive layer 5 is installed so that the barrier adhesive layer 5 overlaps a part of an upper surface of the organic thin-film solar cell and a third barrier layer 7, and a laminate of the barrier adhesive layer 5 and the third barrier layer 7 is installed so that the barrier adhesive layer 5 overlaps a part of a lower surface of the organic thin-film solar cell and the second barrier layer 6. |