发明名称 METHOD FOR HIGH-EFFICIENCY WELDING OF THICK STEEL PLATE
摘要 This method of submerged arc welding includes: a machining step of machining a double V groove; and a welding step of performing a one-run welding with a flux. In the welding step, a welding current for a first electrode is an alternating current with a waveform ratio of 60% or greater and 90% or less, and welding currents for the other electrodes are an alternating current with a waveform ratio of 70% or greater, or a negative direct current. The flux includes, in a mass ratio to a total mass of the flux, 10% to 50% of Al 2 O 3 : and 16% to 30% of SiO 2 , and further includes: one or more of MgO, TiO 2 , CaF 2 , and MnO, a total of which is 10% to 60%, the MgO, TiO 2 CaF 2 , and MnO being limited to not more than 40%, 20%, 30%, and 20%, respectively.
申请公布号 EP2767361(A4) 申请公布日期 2015.09.23
申请号 EP20120849423 申请日期 2012.11.14
申请人 NIPPON STEEL & SUMITOMO METAL CORPORATION 发明人 KOJIMA, KAZUHIRO;NOSE, TETSURO;INOUE, HIROSHIGE
分类号 B23K9/18;B23K9/23;B23K35/30;B23K35/36;B23K35/362;C22C38/00;C22C38/02;C22C38/04;C22C38/08;C22C38/12;C22C38/14 主分类号 B23K9/18
代理机构 代理人
主权项
地址