发明名称 |
HAIRSPRING MATERIAL FOR MECHANICAL TIMEPIECE AND HAIRSPRING USING THE SAME |
摘要 |
[Problem] To provide a hairspring material for a mechanical timepiece, a variation in Young's modulus of which can be made smaller than that of conventional ones. [Solution] The hairspring material for a mechanical timepiece of the present invention comprises an alloy which contains 37.5 to 39.5% by mass of Ni, 9.2 to 9.9% by mass of Cr, 0.35 to 0.55% by mass of Ti and 0.6 to 0.9% by mass of Be, based on the total amount of the alloy, and contains a remainder including Fe and unavoidable impurities, said alloy being an alloy containing, as the unavoidable impurities, C (carbon), Mn in an amount of more than 0% by mass but not more than 0.5% by mass and Al in an amount of more than 0% by mass but less than 0.03% by mass, the amount of said C (carbon) being limited to not more than 0.03% by mass. |
申请公布号 |
US2015241847(A1) |
申请公布日期 |
2015.08.27 |
申请号 |
US201314421233 |
申请日期 |
2013.08.29 |
申请人 |
CITIZEN HOLDING CO., LTD. ;CITIZEN WATCH CO., LTD. ;HITACHI METALS. LTD. ;NEOMAX MATERIALS CO., LTD. |
发明人 |
Hirai Yoshirou;Matsumoto Shinichi;Tsuchiya Kenji;Yamamoto Shinji |
分类号 |
G04B17/06 |
主分类号 |
G04B17/06 |
代理机构 |
|
代理人 |
|
主权项 |
1. A hairspring material for a mechanical timepiece, comprising an alloy which contains 37.5 to 39.5% by mass of Ni, 9.2 to 9.9% by mass of Cr, 0.35 to 0.55% by mass of Ti and 0.6 to 0.9% by mass of Be, based on the total amount of the alloy, and contains a remainder comprising Fe and unavoidable impurities, said alloy being an alloy containing, as the unavoidable impurities, C (carbon), Mn in an amount of more than 0% by mass but not more than 0.5% by mass and Al in an amount of more than 0% by mass but less than 0.03% by mass, the amount of said C (carbon) being limited to not more than 0.03% by mass. |