发明名称 ECO-FRIENDLY QUICK HARDENING REPAIRING MORTAR COMPOSITION USING SEAWEEDS AND CONSTRUCTING METHODS USING THEREOF
摘要 <p>The present invention relates to an eco-friendly rapid hardening mortar composition for repair with seaweed, which comprises: 10 to 60 parts by weight of seaweed; 20 to 80 parts by weight of methylmethacrylate; 10 to 60 parts by weight of a prepolymer; 5 to 30 parts by weight of a curing agent; 10 to 20 parts by weight of calcium sulfoaluminate; 5 to 15 parts by weight of high functional powder; 5 to 10 parts by weight of an antifoaming agent; 1 to 5 parts by weight of an accelerating agent; and 1 to 5 parts by weight of a water reducing agent, with respect to 100 parts by weight of cement, and to a construction method using the same. The eco-friendly rapid hardening mortar composition for repair using seaweed is capable of shortening the construction period by being rapidly hardened during construction and providing sufficient compressive strength, bending strength, bonding strength and durability which are required to be a mortar composition.</p>
申请公布号 KR101547667(B1) 申请公布日期 2015.08.27
申请号 KR20150016767 申请日期 2015.02.03
申请人 DAEHAN HITECH CONSTRUCTION CO., LTD.;KANG, CHANG GU 发明人 LEE, PYOUNG WOEN;KANG, CHANG GU
分类号 C04B28/00;C04B28/02;C04B28/36 主分类号 C04B28/00
代理机构 代理人
主权项
地址