发明名称 FERRITE STAINLESS STEEL AND MANUFACTURING METHOD THEREFOR
摘要 Provided are a ferritic stainless steel having a corrosion resistance at a certain level or more and a temper-color removal performance at a certain level or more and a method for manufacturing the ferritic stainless steel. A used ferritic stainless steel has a composition containing, by mass%, C: 0.001% to 0.030%, Si: 0.03% to 0.30%, P: 0.05% or less, S: 0.01% or less, Cr: more than 22.0% to 28.0%, Mo: 0.2% to 3.0%, Al: 0.01% to 0.15%, Ti: more than 0.30% to 0.80%, V: 0.001% to 0.080%, and N: 0.001% to 0.050%; Mn: 0.05% to 0.30% and Ni: 0.01% to 5.00%, or Mn: 0.05% to 2.00% and Ni: 0.01% to 0.30%; Nb: 0.05% or less as an optional component; and the balance being Fe and inevitable impurities, and the steel has a surface where TiN having a grain diameter of 1 µm or more is distributed at a density of 30 particles/mm 2 or more.
申请公布号 EP2910659(A1) 申请公布日期 2015.08.26
申请号 EP20130849239 申请日期 2013.10.22
申请人 JFE STEEL CORPORATION 发明人 ISHII, TOMOHIRO;ISHIKAWA, SHIN;OGATA, HIROYUKI;OTA, HIROKI
分类号 C22C38/00;B21B1/22;C21D1/26;C21D9/46;C22C38/02;C22C38/04;C22C38/06;C22C38/44;C22C38/46;C22C38/48;C22C38/50;C23G1/08;C25F1/00 主分类号 C22C38/00
代理机构 代理人
主权项
地址