发明名称 |
Polyolefin composition with low CLTE |
摘要 |
The invention relates to novel polyolefin compositions having a low coefficient of thermal expansion (CLTE), high stiffness and high flowability. The novel compositions comprise a heterophasic propylene copolymer, an inorganic filler, an ethylene/alpha-olefin elastomer and at least two different alpha-nucleating agents. |
申请公布号 |
US9115276(B2) |
申请公布日期 |
2015.08.25 |
申请号 |
US200912737380 |
申请日期 |
2009.07.10 |
申请人 |
Borealis AG |
发明人 |
Brandstetter Franz;Maureder Klaus;Tranninger Michael |
分类号 |
C08K5/01;C08L23/10;C08L23/12;C08K3/34;C08K5/00;C08K5/523;C08L23/08;C08L23/14;C08L23/20 |
主分类号 |
C08K5/01 |
代理机构 |
Warn Partners, P.C. |
代理人 |
Warn Partners, P.C. |
主权项 |
1. Polyolefin composition comprising
a. 54-70 wt %, of a heterophasic propylene copolymer comprising
i. 70-90 wt %, based on the weight of the heterophasic propylene copolymer of a propylene homopolymer, andii. 10-30 wt %, based on the weight of the heterophasic propylene copolymer of an ethylene-propylene rubber, b. 2-10 wt % of an ethylene/α-olefin elastomer, the α-olefin being a C4-C10 α-olefin, c. 20-46 wt % of an inorganic filler, and d. at least two different α-nucleating agents in a total amount of 0.0011-2.0 wt %; wherein the heterophasic propylene copolymer and the ethylene/α-olefin elastomer together account for at least 97% of all polymeric components of the polyolefin composition; and wherein the polyolefin composition has a CLTE<60 μm/m.K. |