发明名称 フェライト焼結体および電子部品
摘要 PROBLEM TO BE SOLVED: To provide a ferrite sintered body which ensures a small rate of change in initial permeability in a wide temperature range (-40 to 125°C) and whose initial permeability is in a specific range (about 350 to 700).SOLUTION: A ferrite sintered body has a main component having a spinel structure and including iron oxide, zinc oxide, copper oxide and nickel oxide. The ferrite sintered body has an A phase and a B phase, wherein the A phase is a region in which a content (mol%) of FeOis larger than a content (mol%) of ZnO, and the B phase is a region in which a content (mol%) of FeOis not more than a content (mol%) of ZnO. When FeOin 100 mol% of the main component is represented by x (mol%) and the area ratio of the A phase to the total area of the A phase and the B phase is represented by y (%), (x, y) is within a quadrilateral having the following points A to D as apexes (including portions on the line). Point A (46, 97), point B (46, 83), point C (47.9, 70), point D (47.9, 85).
申请公布号 JP5765250(B2) 申请公布日期 2015.08.19
申请号 JP20120010433 申请日期 2012.01.20
申请人 TDK株式会社 发明人 佐々木 弘勝;伊藤 綱;伊藤 守;川口 達哉;▲高▼木 栄光
分类号 C04B35/30;H01F1/34 主分类号 C04B35/30
代理机构 代理人
主权项
地址