发明名称 Method for removing phosphorus and nitrogen contained in sewage or wastewater using iron ore wastewater
摘要 The present invention provides a method for removing phosphorus and nitrogen contained in sewage or wastewater using iron ore wastewater. According to the method of the present invention, in which the phosphorus and nitrogen contained in sewage or wastewater are crystallized in the form of struvite using iron ore wastewater containing a large amount of Mg2+ produced in a process of upgrading low-grade iron ore and removed, it is possible to reduce the cost of Mg2+ and the cost of iron ore wastewater treatment, thereby earning economic profits. Moreover, it is possible to prevent water pollution by the removal of the phosphorus and nitrogen contained in sewage or wastewater. Furthermore, it is possible to use struvite crystals obtained as a by-product as a time-release compound fertilizer so as to reduce the amount of fertilizer used and the number of fertilizations, thereby reducing soil contamination.
申请公布号 US9102555(B2) 申请公布日期 2015.08.11
申请号 US201113306855 申请日期 2011.11.29
申请人 Korea Institute of Geosciences and Mineral Resources 发明人 Suh Yong Jae;Ju Myung Eun;Kil Dae Sup;Jang Hee Dong
分类号 C02F1/52;C02F1/66;C02F101/10;C02F101/16 主分类号 C02F1/52
代理机构 Bozicevic, Field & Francis LLP 代理人 Field Bret E.;Bozicevic, Field & Francis LLP
主权项 1. A method for removing phosphorus and nitrogen contained in sewage or wastewater using iron ore wastewater, comprising: (1) obtaining iron ore leachate by adding iron ore powder to an acidic solution and stirring the mixture at 90 to 110° C. for 1 to 3 hours; (2) diluting the iron ore leachate with distilled water and separating and discharging residual undissolved powder by centrifugation; (3) adjusting the pH of the iron ore leachate to 7.5 to 9 and obtaining a precipitate of iron hydroxide and a supernatant containing Mg2+ by centrifugation; and (4) adding the supernatant containing Mg2+ obtained in step (3) to a mixed solution of a phosphate (PO43−) solution and an ammonium salt (NH4+) solution, adjusting the pH of the reaction solution to 7.5 to 9, stirring the resulting mixture at room temperature, and removing a precipitate of struvite by filtration, wherein the molar ratio of phosphorus (P) ions to nitrogen (N) ions to magnesium (Mg) ions is 1:3:0.5 to 2.