摘要 |
<p>The present invention relates to a manufacturing method of a functional coffee soap, which comprises: a product of a soap base melted at a temperature of 80°C; coffee powder crushed with the size of 200 micrometer of an average diameter after heating coffee beans at a temperature of 250°C for 10 minutes and 30 seconds and cooling; coffee oil crushed with the size of 200 micrometers of an average diameter and compressed at 550 psi for 10 minutes; and hyaluronic acid put a product mixed with the weight ratio of 100:3:1:1 in a frame, cooled at a temperature of 4°C, and solidified to manufacture a soap.</p> |