发明名称 |
METHOD FOR PURIFYING AL-TI-B ALLOY MELT |
摘要 |
<p>A method for purifying Al -Ti -B) alloy includes putting and melting industrial aluminum ingot in an electromagnetic induction smelting furnace, the melt of Al being covered by a high-temperature covering agent, and its temperature up to at about 670~900°C ; adding material of K 2 TiF 6 and KBF 4 into the smelting furnace and then stirring the compounds therein to react; adding compound comprising Mg, L, Na and F to the evenly stirred K 2 TiF 6 and KBF 4 , the compound having an amount about 0.01%~1% of a sum weight of total K 2 TiF 6 and KBF 4 , and uniformly stirring for about 15~60 minutes under a reaction temperature being constantly at about 670~900°C, the dregs being removed, the Al alloy being casting molded.</p> |
申请公布号 |
EP2530174(B1) |
申请公布日期 |
2015.07.29 |
申请号 |
EP20100723471 |
申请日期 |
2010.05.10 |
申请人 |
SUN XING CHEMICAL & METALLURGICAL MATERIALS (SHENZHEN) CO. LTD. |
发明人 |
CHEN, XUEMIN;YE, QINGDONG;LI, JIANGUO;LIU, CHAOWEN;YU, YUEMING |
分类号 |
C22C1/03;C22B9/10;C22B21/06;C22C1/02;C22C1/06;C22C21/00 |
主分类号 |
C22C1/03 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|