发明名称 Nonwoven web for fastener female member
摘要 A nonwoven web is provided. The nonwoven web contains a side-by-side composite fiber having crimps. The composite fiber contains first and second propylene polymers. The nonwoven web contains a bonded portion that contains a bonding pattern containing zigzag unit patterns. The zigzag unit patterns are continuous and substantially parallel with a first direction and are disposed in a second direction at predetermined intervals. A triangle formed by adjacent three contact points of a first diagonal line and a second diagonal line of the unit pattern contains a part of the unit pattern that is adjacent to the triangle in the second direction.
申请公布号 US9091005(B2) 申请公布日期 2015.07.28
申请号 US200711678282 申请日期 2007.02.23
申请人 MITSUI CHEMICALS, INC. 发明人 Masuda Kazuhiko;Morimoto Hisashi;Horn Thomas Alexander;Kline Mark James
分类号 A61F13/62;D04H1/541;D04H1/4291;D04H3/007;D04H3/02;D04H3/147;D04H1/44;D04H13/00 主分类号 A61F13/62
代理机构 Rankin Hill & Clark LLP 代理人 Rankin Hill & Clark LLP
主权项 1. A receiving component of a fastener including a nonwoven web comprising a composite fiber having crimps, the nonwoven web comprising an embossed portion and a non-embossed portion on only one surface of the nonwoven web, the composite fibers in the embossed portion being bonded by thermal compression by an embossing roll, the composite fibers in the non-embossed portion being capable of engaging with a plurality of hooks of an engaging component, the embossed portion comprising an embossing pattern that comprises a plurality of zigzag unit patterns disposed in a machine direction, each zigzag unit pattern being spaced from each other, the zigzag unit patterns being continuous and parallel with a cross machine direction of the embossing roll, the zigzag unit patterns comprising a plurality of first diagonal lines and a plurality of second diagonal lines that are disposed alternately, the plurality of first diagonal lines being disposed parallel to each other and respective first diagonal lines being inclined to a first side at a same angle to the machine direction, the second diagonal lines being disposed parallel to each other and respective second diagonal lines being inclined to a second side at a same angle to the machine direction, first diagonal lines and second diagonal lines being continuous and connected alternately at an end portion or an adjacent portion to the end portion of the first diagonal lines and second diagonal lines, a triangle formed by adjacent three contact points of a first diagonal line and a second diagonal line adjacent to the first diagonal line of the zigzag unit pattern being overlapped by a part of another zigzag unit pattern that is adjacent to the triangle in the machine direction, where the three contact points are at a location where the first diagonal line and the adjacent second diagonal line connect and at other ends of the first diagonal line and the adjacent second diagonal line, and the triangle is formed when imaginary lines connect the three contact points to each other, the zigzag unit patterns having a ratio of W1/W2 of about 0.1 to about 10, wherein W1 is a width between a first apex on a first side and a second apex on a second side of the zigzag unit pattern in the machine direction and W2 is a width between adjacent contact points of a first diagonal line and a second diagonal line in the cross machine direction, the composite fiber having crimps being a side-by-side composite fiber comprising a first propylene polymer and a second propylene polymer, wherein the first and second propylene polymers are arranged to occupy a first area and a second area of a cross section of the composite fiber, respectively, and extend continuously in a longitudinal direction, and each of the first and second propylene polymers forms at least a portion of peripheral surface continuously along the longitudinal direction of the composite fiber, and a melting point of the first propylene polymer measured by differential scanning calorimetry being higher than a melting point of the second propylene polymer by about 15° C. or more, and a weight ratio of the first propylene polymer to the second propylene polymer being from about 50/50 to about 5/95, wherein an area percentage of the embossed portion to a sum of the embossed portion and the non-embossed portion is in a range of about 20% to about 30%, and the nonwoven web is a spunbonded nonwoven web.
地址 Tokyo JP