<p>The present invention relates to a lane paint composition, comprising: 1-40% wt of an inorganic filler, 60-98.9 wt% of a room temperature curing binder, and 0.01-10 wt% of a curing accelerator, wherein the room temperature curing binder comprises: 40-98 wt% of methyl methacrylate resin, 1-15 wt% of acrylic acid-methyl resin, 0.1-15 wt% of polyurethane resin, 0.1-15 wt% of polystyrene resin, 0.01-15 wt% of epoxy resin, 0.01-10 wt% of dibutyltin dilaurate, 0.01-10 wt% of polyacrylonitrile resin. The lane paint composition is used to paint lanes on asphalt or concrete material; exhibits superior abrasion resistance, durability, and visibility; and provides better visibility at night through high reflectivity for light emitted from a head light on a vehicle.</p> |