摘要 |
<p><P>PROBLEM TO BE SOLVED: To provide a method for efficiently producing an ethylene wax with a narrow molecular weight distribution. <P>SOLUTION: The method for producing an ethylene wax with intrinsic viscosity of 0.60 dL/g or less includes polymerizing ethylene in the presence of an olefin polymerization catalyst including a fourth group transition metal compound represented by general formula (1), a compound which reacts with the fourth group transition metal compound and forms an ion pair, and (C) an organoaluminum compound. <P>COPYRIGHT: (C)2011,JPO&INPIT</p> |