发明名称 BLAST-FURNACE-BLOW-IN CHARCOAL AND METHOD FOR PRODUCING SAME
摘要 In blast-furnace-blow-in charcoal that is blown in from a tuyere to the interior of a blast furnace main body of a blast furnace facility, the oxygen atom content (on a dry basis) is 10-20 wt % and the average pore size is 10-50 nm.
申请公布号 US2015191803(A1) 申请公布日期 2015.07.09
申请号 US201314412921 申请日期 2013.05.15
申请人 MITSUBISHI HEAVY INDUSTRIES, LTD. 发明人 Omoto Setsuo;Nakagawa Keiichi;Hamada Tsutomu;Sakaguchi Masakazu
分类号 C21B5/00;C10B57/10;C10B53/00 主分类号 C21B5/00
代理机构 代理人
主权项 1. Blast furnace injection coal to be blown into a blast furnace main unit of a blast furnace installation through a tuyere, wherein an oxygen atom content ratio (dry base) is between 10 and 20% by weight, and an average pore size is between 10 and 50 nm.