发明名称 |
Method for producing ternesite |
摘要 |
The present invention relates to the production of ternesite clinkers containing 20 to 95% by weight C5S2$ and less than 15% by weight C4A3$, and to the use of ternesite as an additive to hydraulic and/or latent hydraulic and/or pozzolanic materials. |
申请公布号 |
US9073785(B2) |
申请公布日期 |
2015.07.07 |
申请号 |
US201214239348 |
申请日期 |
2012.07.16 |
申请人 |
HEIDELBERGCEMENT AG |
发明人 |
Bullerjahn Frank;Schmitt Dirk;Ben Haha Mohsen |
分类号 |
C04B7/345;C04B7/32;C04B28/06;C04B28/04;C04B28/08;C04B40/00;C04B28/02;C04B22/00;C04B22/14;C04B7/02;C04B7/26;C04B7/28;C04B16/04;C04B103/14;C04B111/00 |
主分类号 |
C04B7/345 |
代理机构 |
Strain & Strain PLLC |
代理人 |
Strain, Esq. Paul D.;Strain & Strain PLLC |
主权项 |
1. A method for producing a ternesite clinker, comprising sintering a raw meal mixture, which contains at least sources for CaO, SiO2, and SO3, wherein a temperature during sintering is adjusted in the range of 900 to 1300° C. such that the ternesite clinker has a content of C5S2$ ranging from 20 to 95% by weight and a content of C4(AxF(1-x))3$, with x being 0.1 to 1, of less than 15% by weight, in each case relative to the total weight of the clinker. |