发明名称 |
Epoxidation process with post-conditioning step |
摘要 |
A method for the epoxidation of an olefin comprising the steps of reacting a feed gas composition containing an olefin, oxygen, and a moderator having a post-conditioning step where the catalyst is exposed to reactor feed having a chlorides concentration of from about 5 ppm to about 7 ppm and at a temperature of about 215° C. to about 225° C. |
申请公布号 |
US9067902(B2) |
申请公布日期 |
2015.06.30 |
申请号 |
US201414152519 |
申请日期 |
2014.01.10 |
申请人 |
Scientific Design Company, Inc. |
发明人 |
Padia Ashok S.;Al-Ahmadi Hassan Eisa |
分类号 |
C07D301/03;C07C43/00;C07C29/00;C07D301/10;C07D301/08;C07C29/10 |
主分类号 |
C07D301/03 |
代理机构 |
Scully, Scott, Murphy & Presser, P.C. |
代理人 |
Scully, Scott, Murphy & Presser, P.C. |
主权项 |
1. A method for the epoxidation of an olefin comprising:
initiating an epoxidation reaction by reacting a feed gas composition containing ethylene, oxygen, and a chloride moderator present at a concentration of from about 0.5 ppm to about 3 ppm, in the presence of an epoxidation catalyst at a temperature of about 245° C. to about 265° C.; increasing the moderator concentration to about 5 ppm to about 7 ppm and lowering the temperature to about 215° C. to about 225° C.; and maintaining the moderator concentration within the range of 5 ppm to about 7 ppm and the temperature in the range of about 215° C. to about 225° C. for a time period of about 50 hours to about 150 hours. |