<p>STEAM TURBINE ROTOR There is provided a steam turbine rotor with high reliability and corresponding to increase in length of a high strength steel blade, in which only a low-pressure last stage is highly strengthened. The steam turbine rotor includes a steam turbine low-pressure last stage long blade made of a precipitation hardening type martensitic stainless steel containing, in mass, 0.1% or less of C, 0.1% or less of N, 9.0% to 14.0% inclusive of Cr, 9.0% to 14.0% inclusive of Ni, 0.5% to 2.5% inclusive of Mo, 0.5% or less of Si, 1.0% or less of Mn, 0.25% to 1.75% inclusive of Ti, 0.25% to 1.75% inclusive of Al, and the balance consisting of Fe and inevitable impurities, and a disk having a specific alloy composition is joined to a last stage section of the turbine rotor made of a low-alloy steel. Fig. 3</p> |