发明名称 フェライト系快削ステンレス鋼およびその製造方法
摘要 <p><P>PROBLEM TO BE SOLVED: To provide an inexpensive, free-cutting ferritic stainless steel that is free of highly toxic heavy metals such as Pb, is excellent in productivity and is excellent in surface accuracy and tool wear resistance in cutting. <P>SOLUTION: The free-cutting ferritic stainless steel contains, by mass%,≤0.030% C,≤1.0% Si,≤2.0% Mn, 0.02-0.10% P, 0.15-0.50% S, 15.0-20.0% Cr,≤0.030% N, 1.0-2.5% Cu and at least one chosen from 0.03-0.50% Sn, 0.02-0.20% Ag and 0.02-0.50% Zn, and includes a secondary phase composed of essentially Cu and at least one chosen from Sn, Ag and Zn in an amount of≥2 mass%. In the secondary phase, ones with a grain size of≥0.01μm are dispersed in a matrix at an area ratio of≥0.2% in a cross-sectional structure of the steel and a Vickers hardness is≥160 Hv. <P>COPYRIGHT: (C)2012,JPO&INPIT</p>
申请公布号 JP5737801(B2) 申请公布日期 2015.06.17
申请号 JP20110022542 申请日期 2011.02.04
申请人 发明人
分类号 C22C38/00;C21D6/00;C22C38/60 主分类号 C22C38/00