摘要 |
The present invention provides a method for producing high-purity calcium, the method being characterized by the following: performing first sublimation purification by introducing calcium starting material having a purity, excluding the gas components, of 4N or less into a crucible of a sublimation vessel, subjecting the starting material to sublimation by heating at 750°C to 800°C, and causing the product to deposit (evaporate) onto the inside walls of the sublimation vessel; and then, once the calcium that has been subjected to first sublimation purification is recovered, performing second sublimation purification by introducing the recovered calcium again to the crucible to the sublimation vessel, heating the recovered calcium at 750°C to 800°C, and causing the product to similarly deposit (evaporate) on the inside walls of the sublimation vessel thereby recovering calcium having a purity of 4N5 or higher It is an object of the present invention to provide a technology with which calcium that has been brought to a high-purity can be obtained with stability to be used for the production of high-purity lanthanum, as well as to be used as a reducing agent for other rare earth elements, a desulfurizing or deoxidizing agent for metals, or a getter for high-vacuum pumps. |