发明名称 Near zero coefficient of thermal expansion of beta-eucryptite without microcracking
摘要 The present invention is drawn to a lithia alumina silica material that exhibits a low CTE over a broad temperature range and a method of making the same. The low CTE of the material allows for a decrease in microcracking within the material.
申请公布号 US9056794(B2) 申请公布日期 2015.06.16
申请号 US201313866883 申请日期 2013.04.19
申请人 发明人 Reimanis Ivar;Ramalingam Subramanian
分类号 C04B35/14;C04B35/00;C04B35/19;C01B33/26;C04B35/624;C04B35/626;C04B35/645 主分类号 C04B35/14
代理机构 Sheridan Ross P.C. 代理人 Sheridan Ross P.C.
主权项 1. A method for producing a doped low thermal expansion lithia alumina silica material, comprising: mixing a source of silica comprising an orthosilicate with an alcohol and a water to produce a first mixture comprising a first volumetric ratio of about 0.5 to about 1.5 parts of the orthosilicate to about 1.0 parts of the alcohol, and a second volumetric ratio of about 0.1 to about 1.0 parts of the water to about 1.0 part of the orthosilicate; adjusting the pH of the first mixture to between about 0.5 and about 4.0 by addition of an acid to produce a pH adjusted mixture; modifying the pH adjusted mixture by adding a source of alumina comprising an aluminum salt, adding a source of lithia comprising a lithium salt, and adding a metal salt, wherein the metal salt comprises a metal and a counter-ion, to produce a suspension comprising an elemental ratio of about 1 part of aluminum to about 1 part silicon to about 1 part lithium, and a metal concentration in the range of about 0.01 mole % to about 10 mole % of the metal, wherein the metal concentration is relative to the total amounts of the lithium in the suspension; and processing the suspension to produce the doped low thermal expansion lithia alumina silica material.
地址