发明名称 Método para a produção de um tubo de aço sem costura de alta liga
摘要 <p>Pipe-swelling can be prevented by piercing-rolling a high-alloy steel billet heated to a temperature range from 900 to 1250°C with a piercing mill equipped with main rolls having a surface roughness R max of 150 to 500 µm. A ratio (the gap W G of guide rolls/the gap W R of the main rolls) is preferably at 1.10 to 1.20. The difference (¸ P - ¸ R ) is preferably set at 0 to 3.0°, where ¸ R is an angle between an exit-side face of each of the main rolls of the piercing mill and the pass line; and ¸ P is an angle between a rolling face of the piercing plug and the pass line.</p>
申请公布号 BRPI0822466(A2) 申请公布日期 2015.06.16
申请号 BR2008PI22466 申请日期 2008.12.04
申请人 SUMITOMO METAL INDUSTRIES, LTD. 发明人 KENICHI SAITOU
分类号 B21B19/04;B21B27/00;B21B27/02;B21B27/10 主分类号 B21B19/04