发明名称 |
THERMOPLASTIC POLYCARBONATE RESIN COMPOSITION |
摘要 |
A thermoplastic polycarbonate resin composition may include about 50 to about 70 wt % of a polycarbonate resin; about 5 to about 20 wt % of a vinyl cyanide compound-conjugated diene-vinyl aromatic hydrocarbon copolymer; about 10 to about 30 wt % of a polyester resin; about 3 to about 15 wt % of a maleimide-based copolymer; about 2 to about 10 wt % of an impact modifier; and about 0.1 to about 1.0 wt % of a nucleating agent, wherein the polycarbonate resin has a melt index of about 2 to about 20 g/10 min (300° C., 2.16 kg). The thermoplastic polycarbonate resin composition has excellent chemical resistance and mechanical properties. |
申请公布号 |
US2015159013(A1) |
申请公布日期 |
2015.06.11 |
申请号 |
US201414322585 |
申请日期 |
2014.07.02 |
申请人 |
HYUNDAI MOBIS CO., LTD. ;LG CHEM. LTD. |
发明人 |
Chang Jae Joon;Kim Hyeon Don;Chun Yong;Kim Myeung Il;Choi Jong Kuk;Kim Yong;Lee Sung Ho;Ok Dae Yong |
分类号 |
C08L69/00 |
主分类号 |
C08L69/00 |
代理机构 |
|
代理人 |
|
主权项 |
1. A thermoplastic polycarbonate resin composition comprising:
about 50 to about 70 wt % of a polycarbonate resin; about 5 to about 20 wt % of a vinyl cyanide compound-conjugated diene-vinyl aromatic hydrocarbon copolymer; about 10 to about 30 wt % of a polyester resin; about 3 to about 15 wt % of a maleimide-based copolymer; about 2 to about 10 wt % of an impact modifier; and about 0.1 to about 1.0 wt % of a nucleating agent, wherein the polycarbonate resin has a melt index of about 2 to about 20 g/10 min (300° C., 2.16 kg). |
地址 |