发明名称 PRETREATMENT METHOD OF COPPER-CONTAINING MOLYBDENITE
摘要 <p>PROBLEM TO BE SOLVED: To provide a pretreatment method of copper-containing molybdenite that removes copper alone while minimizing oxidation of molybdenum in reacting low-grade molybdenite containing copper sulfide with sulfuric acid to produce ferromolybdenum for steel making.SOLUTION: Before pretreatment, molybdenite is subjected to ore flotation to separate minerals on the hydrophilic surface leaving the minerals in a solution, and further may be subjected to crushing and granulating to improve reactivity with sulfuric acid. The pretreatment includes a step for mixing the copper-containing molybdenite with sulfuric acid at an equivalence ratio of 0.9-1.8, a step for heating and subjecting the mixture to sulfation reaction at 180-240°C for 20-80 minutes, a step for water exudation by adding water and agitating after the sulfation reaction, a step for separating a solid from a liquid after the water exudation, and a step for drying the separated solid.</p>
申请公布号 JP2015105436(A) 申请公布日期 2015.06.08
申请号 JP20130258499 申请日期 2013.12.13
申请人 KOREA INSTITUTE OF GEOSCIENCE AND MINERAL RESOURCES 发明人 CHOI YOUNG YOON;SHIN SHUN MYUNG;NAM CHUL WOO;KIM HYUNG SUK
分类号 C22B3/04 主分类号 C22B3/04
代理机构 代理人
主权项
地址