发明名称 液晶性樹脂組成物
摘要 <p>Provided is a technique whereby the measuring time of a liquid crystalline resin composition containing glass fibers can be shortened and stabilized and the cushion content thereof can be reduced and stabilized while sustaining the good physical properties of the composition. To a mixture comprising a liquid crystalline resin and glass fibers, glass beads are further added in an amount of 4 mass% to 7 mass % relative to the total mass of the liquid crystalline resin composition.  It is particularly preferable to add the glass fibers in an amount of 20 mass% to 40 mass % relative to the total mass of the liquid crystalline resin composition.  Thus, the measuring time of the liquid crystalline resin composition containing glass fibers can be shortened and stabilized and the cushion content thereof can be reduced and stabilized while sustaining the good physical properties of the composition even in the case of injection molding using a liquid crystalline resin material having a high melting point and a low viscosity.</p>
申请公布号 JP5727229(B2) 申请公布日期 2015.06.03
申请号 JP20100542000 申请日期 2009.12.04
申请人 发明人
分类号 C08L67/03;C08K7/14;C08K7/20 主分类号 C08L67/03
代理机构 代理人
主权项
地址