发明名称 Blends of polyphenylene ether sulfone and silicone polyester carbonate
摘要 Disclosed herein is a composition comprising a polyphenylene ether sulfone and a resorcinol based silicone aryl polyester carbonate copolymer wherein greater than or equal to 50 mol % of copolymer repeating units are ester units derived from resorcinol, based on the total molar amount of all repeating units in the polymer and wherein the blend has less than 1 weight percent polycarbonate, based on the total weight of the composition, has FAR 25.853 peak heat release of less than 60 KW/m2 and time to peak heat release of greater than or equal to 120 seconds.
申请公布号 US9045640(B2) 申请公布日期 2015.06.02
申请号 US201314047508 申请日期 2013.10.07
申请人 SABIC GLOBAL TECHNOLOGIES B.V. 发明人 Gallucci Robert Russell;Sybert Paul Dean
分类号 C08L83/04;C08K5/55;C08K3/38;C08F283/08;C08L73/00;C08G18/67;C08L51/00;C08L69/00;C08G75/02;C08L81/00;C08F283/00;C08G63/08;C08L81/06;C08L27/18;C08L71/08 主分类号 C08L83/04
代理机构 Cantor Colburn LLP 代理人 Cantor Colburn LLP
主权项 1. An article comprising a thermoplastic composition, wherein the article is a rail car interior article or an airplane interior article and the thermoplastic composition consists of 70 to 99 wt % of a polyphenylene ether sulfone, 1 to 30 wt % of a resorcinol based silicone aryl polyester carbonate copolymer, based on the total weight of the composition, and optionally a metal oxide, fluoropolymer, boron compound, brominated flame retardant, antioxidant, colorant, light stabilizer, optical brightener, UV absorber, flow aid, mold release agent, reinforcing filler, or a combination thereof, wherein greater than or equal to 50 mol % of resorcinol based silicone aryl polyester carbonate copolymer repeating units are ester units derived from resorcinol, based on the total molar amount of all repeating units in the polymer and wherein the blend comprises less than 1 weight percent polycarbonate, based on the total weight of the composition, and the composition has a FAR 25.853 peak heat release of less than 50 KW/m2, a time to peak heat release of greater than or equal to 120 seconds, and a melt volume viscosity rate (MVR) at 300° C. using a six minute equilibration time, with 6.7 Kg, as measured by ASTM D1238, of greater than or equal to 2.0 cc/10 minutes.