发明名称 OPHTHALMIC LENS COMPRISING A BASE OF POLYMERIC MATERIAL WITH A COATING HAVING AN INTERFERENTIAL, ANTI-REFLECTIVE, ANTI-IRIDESCENT AND IR FILTER MULTIPLE LAYER STRUCTURE
摘要 Ophthalmic lens including a base of polymeric material with a coating having an interferential, anti-reflective, anti-iridescent and infrared filter multiple layer structure. An interphase, a first layer (of 91-169 nm) with a refraction index higher than 1.8, a second layer (of 128-248 nm) with a refraction index lower than 1.65, a third layer (of 73-159 nm) with a refraction index higher than 1.8 and a fourth layer (of 40-138 nm) with a refraction index lower than 1.8. A total thickness of the multiple layer structure is less than 600 nm. The structure can have intermediate layers with intermediate refraction indices, in which case a doublet of two adjacent layers that fulfil the thicknesses above is replaced by a triplet so that the thickness and an optical thickness of the triplet differ from those of the doublet by less than 5%, respectively.
申请公布号 US2015146161(A1) 申请公布日期 2015.05.28
申请号 US201414553428 申请日期 2014.11.25
申请人 INDO OPTICAL S.L. 发明人 RIGATO Franco;Casanellas Peñalver Glòria;Artús colomer Del Vallès Pau;Vilajoana Mas Antoni;Dürsteler López Juan Carlos
分类号 G02C7/10;G02B1/14 主分类号 G02C7/10
代理机构 代理人
主权项 1. Ophthalmic lens having a base of polymeric material with a coating having an interferential multiple layer structure, comprising: an interphase, orientated towards the base, of a material from the group made up of SiOx, SiO2, Cr, Ni/Cr, SnO2, Al2O3, AlN, ZnO, SiO/Cr, SiOx/Al2O3, ITO, MoO3, with a thickness between 0 and 150 nm, a first high refraction index layer, of a material from the group made up of oxides, nitrides or oxynitrides of Zr, Ti, Sb, In, Sn, Ta, Nb, Hf and mixtures thereof, with a refraction index nD higher than 1.8, a second low refraction index layer, of a material from the group made up of SiO2, MgF2, Al2O3, LaF3 and mixtures thereof, with a refraction index nD lower than 1.65, a third high refraction index layer of a material from the group made up of oxides, nitrides or oxynitrides of Zr, Ti, Sb, In, Sn, Ta, Nb, Hf and mixtures thereof, with a refraction index nD higher than 1.8, a fourth layer, of a material from the group made up of SiO2, MgF2, Al2O3, LaF3 and mixtures thereof, with a refraction index nD lower than 1.8, where between the interphase and the first high refraction index layer there is a first intermediate layer with a refraction index nD lower than 1.8 and with a thickness between 0 and 160 nm, where between the first high refraction index layer and the second low refraction index layer there is a second intermediate layer with a refraction index nD between 1.65 and 1.8 and with a thickness between 0 and 100 nm, where between the second low refraction index layer and the third high refraction index layer there is a third intermediate layer with a refraction index nD between 1.65 and 1.8 and with a thickness between 0 and 110 nm, where a total thickness of said multiple layer structure is at the most 600 nm, measured from a start of the interphase to an end of the fourth layer, and where, if there is none of said intermediate layers, the thickness of said first high refraction index layer is between 91 and 169 nm, preferably between 101 and 159 nm, the thickness of said second low refraction index layer is between 128 and 248 nm, preferably entre 138 and 240 nm, the thickness of said third high refraction index layer is between 73 and 159 nm, preferably between 83 and 147 nm, and the thickness of said fourth layer is between 40 and 138 nm, and, if there is one of said intermediate layers, it holds that: the doublet made up of the first high refraction index layer and the second low refraction index layer that fulfil said thicknesses is replaced by a triplet made up of a first intermediate layer, a first high refraction index layer and a second low refraction index layer such that the thickness of said triplet differs from the thickness of said doublet by less than 5%, and such that the optical thickness of said triplet differs from the optical thickness of said doublet by less than 5%, and/or the doublet made up of the first high refraction index layer and the second low refraction index layer which fulfil said thicknesses is replaced by a triplet made up of a first high refraction index layer, a second intermediate layer and a second low refraction index layer such that the thickness of said triplet differs from the thickness of said doublet by less than 5%, and such that the optical thickness of said triplet differs from the optical thickness of said doublet by less than 5%, and/or the doublet made up of the second low refraction index layer and the third high refraction index layer which fulfil said thicknesses is replaced by a triplet made up of a second low refraction index layer, a third intermediate layer and a third high refraction index layer such that the thickness of said triplet differs from the thickness of said doublet by less than 5%, and such that the optical thickness of said triplet differs from the optical thickness of said doublet by less than 5%.
地址 Barcelona ES