发明名称 |
Poly(phenylene ether) copolymer and method of making |
摘要 |
A poly(phenylene ether) copolymer comprises about 5 to 40 mole percent repeat units derived from 2-phenylphenol and 60 to about 95 mole percent repeat units derived from 2,6-dimethylphenol, wherein the poly(phenylene ether) copolymer has a weight average molecular weight of at least 8,000 atomic mass units, as measured by gel permeation chromatography. A method of preparing the poly(phenylene ether) copolymer, comprises oxidatively copolymerizing a monomer mixture comprising about 5 to 40 mole percent 2-phenylphenol and about 60 to about 95 mole percent 2,6-dimethylphenol in the presence of a solvent, molecular oxygen, and a polymerization catalyst comprising a metal ion and at least one amine ligand to form a solution of the poly(phenylene ether) copolymer in the solvent, wherein a ratio of total moles of 2-phenylphenol and 2,6-dimethylphenol to moles of metal ion is about 10:1 to about 1200:1. |
申请公布号 |
US9018342(B2) |
申请公布日期 |
2015.04.28 |
申请号 |
US201213881480 |
申请日期 |
2012.07.27 |
申请人 |
Sabic Global Technologies B.V. |
发明人 |
Carrillo Alvaro;Fisher Scott Michael;Guo Hua;Moyses Stephan;Tarkin-Tas Eylem |
分类号 |
C08G65/38;C08G65/44;C08L71/12;C08G65/46;C08G65/40 |
主分类号 |
C08G65/38 |
代理机构 |
Cantor Colburn LLP |
代理人 |
Cantor Colburn LLP |
主权项 |
1. A poly(phenylene ether) copolymer comprising about 5 to 40 mole percent repeat units derived from 2-phenylphenol and 60 to about 95 mole percent repeat units derived from 2,6-dimethylphenol,
wherein the poly(phenylene ether) copolymer has a weight average molecular weight of 8,000 to about 200,000 atomic mass units, as measured by gel permeation chromatography; and wherein the poly(phenylene ether) copolymer comprises:
a mole percent of 2-phenylphenol head units based on 100 mole percent total 2-phenylphenol head units and 2,6-dimethylphenol head units, anda total mole percent of 2-phenylphenol repeat units, based on 100 mole percent total 2-phenylphenol repeat units and 2,6-dimethylphenol repeat units,wherein the mole percent of 2-phenylphenol head units is greater than the total mole percent of 2-phenylphenol repeat units; and wherein the poly(phenylene ether) copolymer is prepared by a process comprising: oxidatively copolymerizing a monomer mixture comprising about 5 to 40 mole percent 2-phenylphenol and about 60 to about 95 mole percent 2,6-dimethylphenol in the presence of a solvent, molecular oxygen, and a polymerization catalyst comprising a metal ion and at least one amine ligand to form a solution of the poly(phenylene ether) copolymer in the solvent, wherein a ratio of total moles of 2-phenylphenol and 2,6-dimethylphenol to moles of metal ion is about 20:1 to about 200:1; and wherein a ratio of moles of amine groups in the amine ligands to moles metal ion is about 1:1 to about 5:1. |
地址 |
NL |