摘要 |
<p> A fingerprint-resistant anti-reflection film having a hard coat layer, a high-refractive-index layer, and a low-refractive-index layer laminated in the stated order on one side of a transparent base film. The refractive index of the high-refractive-index layer is 1.50-1.65, and the film thickness thereof is 130-180 nm. The refractive index of the low-refractive-index layer is 1.36-1.42, and the film thickness thereof is 70-100 nm. The minimum reflectance wavelength (λ(min)) in a wavelength range of 350-850 nm is 350-530 nm, and the wavelength (λ(bend)) at the bending point in the wavelength range of 350-850 nm satisfies the relationship λ(min) < λ(bend). Furthermore, the luminous reflectance of the fingerprint-resistant anti-reflection film is 2.0% or lower, the reflection chroma (C) is less than 6.0, and the reflection color difference (△E) before and after adhesion of sebum soil is less than 7.0.</p> |