GROUND SOLIDIFICATION METHOD |
摘要 |
<p>PROBLEM TO BE SOLVED: To provide a method for solidifying the ground in a short time even in winter even if there is a puddle in the ground and even if there is meandering, and for stabilizing the ground by spraying solidification material slurry in a constant thickness.SOLUTION: A ground solidification method is provided so that a solidification material of including a coagulation conditioner of 0-1 pt.mass to a solidification material of 100 pts.mass of including cement and/or blast furnace slag powder of 100 pts.mass and amorphous calcium aluminate powder of 10-50 pts.mass of the CaO/AlOmolar ratio of 1.7-3.0, is pneumatically force-fed by compressed air, and water of 70-300 pts.mass is continuously supplied to the solidification material of 100 pts.mass on the tip of a solidification material supply pipe, and solidification material slurry is prepared, and the prepared solidification slurry is sprayed on a farmland surface from a discharge pipe hose, and the ground is solidified.</p> |
申请公布号 |
JP2015074896(A) |
申请公布日期 |
2015.04.20 |
申请号 |
JP20130210737 |
申请日期 |
2013.10.08 |
申请人 |
DENKI KAGAKU KOGYO KK;NATIONAL AGRICULTURE & FOOD RESEARCH ORGANIZATION |
发明人 |
TERAJIMA ISAO;OKUYAMA KOJI;WATANABE AKIRA;ITO KAZUYUKI;HARAGUCHI NOBUAKI;WAKASUGI KOSUKE |
分类号 |
E02D3/12;A01M21/00;C04B22/08;C04B22/10;C04B22/16;C04B24/06;C04B24/38;C04B28/02;C04B28/08;C09K17/02;C09K17/06;C09K17/08;C09K17/10;C09K17/14;C09K17/44;G21F9/00;G21F9/28;G21F9/30 |
主分类号 |
E02D3/12 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|