摘要 |
<p>PROBLEM TO BE SOLVED: To provide a blow-molding container which can suppress the occurrence of a defect such as gel-like fish-eyes and streaks due to fusion molding, coloration and smell, has superior appearance, permits satisfactory self-purging property of EVOH-containing resin composition to be used, has quality of adequate strength, etc., and can be manufactured at a low cost.SOLUTION: A blow molding container includes a first layer 1 which consists essentially of ethylene-vinylalcohol copolymer (I) and a second layer and so on 2 to 4 made of thermoplastic resin if desired. Therein, the first layer contains saturated ketone (II) and the content of the saturated ketone (II) in the first layer is 0.01 to 100 ppm.</p> |