发明名称 steel furniture powder coating functionality an added healing ceramic composition
摘要 <p>The present invention relates to a functional healing ceramic composition added to coating paint powders used for steel furniture, comprising 68.0-85.0 wt% of silicon dioxide; 5.0-9.0 wt% of alumina; 1.9-4.5 wt% of iron sesquiozide; 1.9-4.5 wt% of calcium oxide; 0.1-1.0 wt% of magnesium oxide; 3.0-6.0 wt% of potassium oxide; 2.0-6.0 wt% of sodium oxide; and 0.1-1.0 wt% of titanium dioxide, wherein the functional healing ceramic composition added to coating paint powders used for steel furniture radiates far infrared rays and accordingly enables people to get their vibration rhythm; restores original power of the human body and accordingly strengthens immunity and facilities blood circulation; activates tissues of the human body and accordingly removes oxygen free radicals; and has effects of safely discharging waste products and carbon dioxide out of the human body by facilitating metabolism and removing hangovers and fatigues.</p>
申请公布号 KR101512595(B1) 申请公布日期 2015.04.15
申请号 KR20140090016 申请日期 2014.07.16
申请人 发明人
分类号 C04B35/03;C04B35/14;C04B35/18;C04B35/22 主分类号 C04B35/03
代理机构 代理人
主权项
地址