发明名称 Apparatus for preparing pellets of poly(trimethylene terephthalate)
摘要 An apparatus is described having an extrusion means for extruding a molten polymer strand; a pelletizer; and a trough disposed to convey a polymer strand from the extrusion means to the pelletizer; the trough has an interior bottom surface; a water dispensing means disposed to provide a layer of water on a first portion of the interior bottom surface that is proximate to the extrusion means; a mesh or perforated surface disposed in the trough downstream from the water dispensing means, disposed to permit the separation of water from a water-immersed strand incident upon it; and a second portion of the interior bottom surface downstream from that mesh or perforated surface, disposed to contain a layer of water.
申请公布号 US8992198(B2) 申请公布日期 2015.03.31
申请号 US201213405387 申请日期 2012.02.27
申请人 E I du Pont de Nemours and Company 发明人 Madeleine Dennis Gerard;Molitor Michael Joseph;Eng John Harvey
分类号 B29B9/06;B29C47/88;B29C47/00;B29C47/30 主分类号 B29B9/06
代理机构 代理人
主权项 1. An apparatus comprising (a) an extrusion means for extruding a molten polymer strand; (b) a pelletizer; and, disposed between said extrusion means and said pelletizer c) a single downward inclined trough, said trough having a plurality of regions comprising i) a first quench region proximate to and downstream from said extrusion means, said first quench region comprising (A) a first trough segment; and,(B) a water dispensing means disposed to provide water to said trough segment;ii) an annealing region downstream from and proximate to said first quench region, said annealing region comprising a mesh or perforated surface disposed just above the water surface to permit the separation of water from a water-immersed polymer strand incident upon it; said mesh or perforated surface disposed such that the water so separated will flow through the mesh or perforated surface back into said trough; said mesh or perforated surface having an adjusted length to provide a strand residence time of 0.3 to 5 seconds upon said mesh or perforated surface. and,iii) a second quench region downstream from said annealing region, said second quench region comprising a second trough segment disposed to contain a layer of water.
地址 Wilmington DE US