发明名称 SINGLE-FIRE TWO-STEP SOAK METHOD
摘要 <p>A method for making a cordierite filter article, including: firing an extruded green body batch composition according to: a first temperature ramping from ambient temperature up to a first soaking temperature; a first soaking at a temperature of at least 1255° C. for at least 2 hours; a second temperature ramping from the first soak temperature down to a second soak temperature; and a second soaking at a temperature of at least 1250° C. and at least 5° C. below the first soaking temperature, as defined herein.</p>
申请公布号 EP2850040(A1) 申请公布日期 2015.03.25
申请号 EP20130725516 申请日期 2013.05.10
申请人 CORNING INCORPORATED 发明人 BRONFENBRENNER, DAVID J.;HEPBURN, LISA LARAE;IYER, SRIRAM RANGARAJAN;KUANDYKOV, LEV LVOVITCH;ST. JULIEN, DELL JOSEPH;WHITE, ELIZABETH ANNE
分类号 C04B35/195 主分类号 C04B35/195