发明名称 METHOD OF MANUFACTURING SOFT MAGNETIC CORE
摘要 PROBLEM TO BE SOLVED: To provide a method of manufacturing a soft magnetic core superior in soft magnetic properties and capable of preventing deposition of an Fe compound.SOLUTION: The method of manufacturing a soft magnetic core includes the steps of: forming a layer of an endothermic reaction material 3 the endothermic reaction temperature of which is in a range of a first crystallization temperature and a second crystallization temperature of an amorphous alloy thin band 2 on at least one surface of the amorphous alloy thin band 2; and heat-treating a core formed with an amorphous alloy thin band 2 in which a layer of the endothermic reaction material 3 is laminated; to thereby produce a soft magnetic core 1.
申请公布号 JP2015056424(A) 申请公布日期 2015.03.23
申请号 JP20130187092 申请日期 2013.09.10
申请人 NEC TOKIN CORP 发明人 URATA KENRI;SATAKE KAORU
分类号 H01F41/02;C21D8/12;C21D9/00;C22C38/00;H01F1/153;H01F27/24 主分类号 H01F41/02
代理机构 代理人
主权项
地址