发明名称 |
POLYAMIDE RESIN COMPOSITION AND MANUFACTURING METHOD THEREOF |
摘要 |
<p>PROBLEM TO BE SOLVED: To provide a polyamide resin composition not only securing sufficient mechanical properties, but also excellent in surface appearance of a molded body and internal smoothness when made as a blow molded body, and to provide a manufacturing method thereof.SOLUTION: The polyamide resin composition contains (A) a polyamide resin of 25 mass% to 85 mass% and (B) a glass fiber of 15 mass% to 75 mass%. Further a ratio of a weight average fiber length X(μm) of (B) the glass fiber in the polyamide resin composition and a median value D(Y) (μm), (X/Y) is 1.6 or more.</p> |
申请公布号 |
JP2015054916(A) |
申请公布日期 |
2015.03.23 |
申请号 |
JP20130188728 |
申请日期 |
2013.09.11 |
申请人 |
ASAHI KASEI CHEMICALS CORP |
发明人 |
WAKITA TAKAYUKI;SAKUMA TERUAKI;TERADA KAZUNORI |
分类号 |
C08L77/00;C08J5/04;C08K7/14 |
主分类号 |
C08L77/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|